Conversation-specific knowledge extracted from the drying tpu for printing discussion.
EXTRACTED KNOWLEDGE / HOW-TO FROM CONVERSATION
QUESTION / CONTEXT: Still getting g stringing issues. How long and at what temp would you dry this before printing in the creator 5 pro?
- 55°C / 131°F for 6 hours as the starting point.
- If it's been sitting exposed for quite a while, go 8–10 hours.
- If it's *really* wet—popping/hissing at the nozzle or producing rough/fuzzy extrusion—I'd give it 10–12 hours.
- I wouldn't exceed about 60°C / 140°F unless EONO3D specifically says the spool can handle it.
- *For this spool tonight: 55°C/131°F × 6 hours. Then run a small stringing test before changing anything else. If you send me your current Creator 5 Pro TPU settings, I can tell you exactly what I'd change after it's dry. [embedded media omitted]
- Open it and load it directly into the Creator 5 Pro.
- Print the same stringing test you're using now with the same settings.
- If the new spool strings dramatically less, we've basically confirmed moisture is the problem with your current TPU.
SPECIFICATION
SourceSupplied ChatGPT export
CategoryBuild & Tools
Conversation2 user turns / 2 assistant turns
Attachments7 references detected
Public detailExtracted knowledge + excerpts
DEVELOPMENT HISTORY
2026.08.31EXPORT-04Matched to the supplied export; key guidance is surfaced separately and the raw transcript remains unpublished.